crusher/mill parts: bimetal thermal composite crusher hammer, blow bar, jaw plate. OEM in China. National patent products.
Port: shanghai
Minimum Order Quantity: 5 Set/Sets OEM welcome
Supply Ability: 200 Ton/Tons per Day special arrange is OK
Payment Terms: L/C,T/T
Contact SupplierPackaging Detail: Sea worthy packing
Delivery Detail: 20 days after receiving the deposit
Crusher/mill parts: bimetal thermal composite crusher hammer, blow bar,jaw plate. casting parts. OEM in China.
1. bimetal composite hammer: duration up to2-3 times of the traditional a single material, and especially for large ball mill line
2. Our patent products with independent research and development (China Patent No. 200810049101.2) --- Bimetal thermal-composite material
3. This product adopts special and professional process and method to combine two different performance of material in molten condition at the same time to melt as a whole one. The interface of combining is up to 100%.
4. The hardness of bimetal thermal-composite material is up to HRC62-65.
5. Its impact ductility is over (AK) 30J/cm2.
6. It has high anti-friction effects and reliable security.
7. the effect of bimetal thermal-composite material is 2-3 times of high manganese material.
8. It is especially used to the hammer and board hammer of large crushers and the lining plate of large ball mill, Remarkable effects particularly when worked in harsh environment of mining conditions, for many crushing field as limestone, cement clinker, sand stone, coal spoil, basalt etc.
The Components of Hammer Head
Chemical Name | C | Mn | Cr | Mo | Ni | Cu | Si | Re |
Chemical Ratio(%) | 2.90 | 0.83 | 19.80 | 0.64 | 0.42 | 0.80 | 0.70 | 0.30 |
The Components ofHammer Body
Chemical Name | C | Mn | Si | |||||
Chemical Ratio(%) | 0.33~0.36 | 0.60~0.80 | 0.4~0.5 |